Wear-resistant cast iron

Wear Resistant Cast Iron (high-Cr) Castings Specific Parameters

The material grade of vary standard which we can produce

GB/T8263 ASTM A532M NF A32-401 DIN1695 BS4844 Trade name
KmTBNi4Cr2-DT 1B   G-X260NiCr4 2 2A Ni-hard 2
KmTBNi4Cr2GT 1A   G-X330NiCr4 2 2B Ni-hard 1
KmTBCr9Ni5 1D FBCr9Ni5 G-X300CrNiSi9 5 2 2C+2D+2E Ni-hard 4
KmTBCr15Mo IIC FBCr15MoNi G-X300CrMo15 3 3A+3B 15-3 alloy
      G-X300CrMoNi15 2 1 3A+3B 15-2-1 alloy
KmTBCr20Mo IID FBCr20MoNi G-X260CrMoNi202 1 3C 20-2-1 alloy
  III A Cr25%   G-X260Cr27 3D  
KmTBCr26 III A Cr25% FBCr26MoNi G-X300CrMo271 3E  

Process Parameters 

Produce Process  Casting Tolerance Weight Range
Resin sand casting  CT10 – CT12 10KGS – 8000KGS
Lost foam (EPC) casting CT8 – CT10 50KGS – 1000KGS
Hard Precision Shell Casting CT8 – CT10 50KGS – 1000KGS

 